| Order | Test Name | Result | Exam Conditions | |
|---|---|---|---|---|
| 1 | State Physical Properties |
Hardness(HS) | 60 | 170℃×10min |
| Tensile Strength(Kg/㎠) | 112 | |||
| Elongation Rate(%) | 422 | |||
| 2 | Heat Resistance Test | Hardness Change Rate(HS) | 3 | 70℃×70hrs |
| Tensile Strength Change Rate(Kg/㎠) | -6.3% | |||
| Elongation Rate Change(%) | -10.2% | |||
| 3 | Compression Permanent Shrinkage Rate(%) | 16.4% | 70℃×22hrs Production 170℃ * 40min |
|
| 4 | Ozone Resistance Test | NO CRACK | 40℃×50pphm×72hrs 20% Elongation |
|