| Order | Test Name | Result | Exam Conditions | |
|---|---|---|---|---|
| 1 | State Physical Properties |
Hardness(HS) | 41 | 170℃×10min |
| Tensile Strength(Kg/㎠) | 113 | |||
| Elongation Rate(%) | 566 | |||
| 2 | Heat Resistance Test |
Hardness Change Rate(HS) | 10 | 125℃×70hrs |
| Tensile Strength Change Rate(Kg/㎠) | -16.8% | |||
| Elongation Rate Change(%) | -29.5% | |||
| Hardness Change Rate(HS) | 4 | 100℃×70hrs | ||
| Tensile Strength Change Rate(Kg/㎠) | -19.1% | |||
| Elongation Rate Change(%) | -23.7% | |||
| 4 | Compression Permanent Shrinkage Rate(%) | 25.5% | 100℃×24hrs Production 170℃ * 40min |
|
| 13.5% | 70℃×24hrs Production 170℃ * 40min |
|||