| Order | Test Name | Result | Exam Conditions | |
|---|---|---|---|---|
| 1 | State Physical Properties |
Hardness(HS) | 65 | 170℃×5min |
| Tensile Strength(Kg/㎠) | 194 | |||
| Elongation Rate(%) | 426 | |||
| 2 | Heat Resistance Test |
Hardness Change Rate(HS) | 6 | 100℃×168hrs |
| Tensile Strength Change Rate(Kg/㎠) | -23.2% | |||
| Elongation Rate Change(%) | -24.8% | |||
| 3 | Compression Permanent Shrinkage Rate(%) | 15.4% | 100℃×22hrs Production 170℃ * 40min |
|
| 4 | Ozone Resistance Test | NO CRACK | 40℃×50pphm×72Hr×20% | |