| Order | Test Name | Result | Exam Conditions | |
|---|---|---|---|---|
| 1 | State Physical Properties |
Hardness(HS) | 60 | 170℃×10min |
| Tensile Strength(Kg/㎠) | 165 | |||
| Elongation Rate(%) | 686 | |||
| 2 | Heat Resistance Test |
Hardness Change Rate(HS) | 5 | 150℃×70hrs |
| Tensile Strength Change Rate(Kg/㎠) | -15.2% | |||
| Elongation Rate Change(%) | -46.2% | |||
| 3 | Compression Permanent Shrinkage Rate(%) | 59.8% | 150℃×22hrs Production 170℃ * 40min |
|
| 4 | Ozone Resistance Test | NO CRACK | 40℃×50pphm×72Hr 20% Elongation |
|