| Order | Test Name | Result | Exam Conditions | |
|---|---|---|---|---|
| 1 | State Physical Properties |
Hardness(HS) | 40 | 170℃×10min |
| Tensile Strength(Kg/㎠) | 105 | |||
| Elongation Rate(%) | 724 | |||
| 2 | Heat Resistance Test |
Hardness Change Rate(HS) | 5 | 70℃×70hrs |
| Tensile Strength Change Rate(Kg/㎠) | 11.4% | |||
| Elongation Rate Change(%) | -8.3% | |||
| 3 | Compression Permanent Shrinkage Rate(%) | 16% | 70℃×22hrs Production 170℃ * 40min |
|