| Order | Test Name | Result | Exam Conditions | |
|---|---|---|---|---|
| 1 | State Physical Properties |
Hardness(HS) | 72 | 170℃×10min 2nd Vulcanization 150℃×2Hr |
| Tensile Strength(N/㎠) | 157 | |||
| Elongation Rate(%) | 211 | |||
| 2 | Heat Resistance Test |
Hardness Change Rate(HS) | 3 | 100℃×200hrs |
| Tensile Strength Change Rate(Kg/㎠) | -1.3% | |||
| Elongation Rate Change(%) | -4.1% | |||
| 3 | Compression Permanent Shrinkage Rate(%) | 4.9% | 100℃×72hrs Specimen Preparation Methods 170℃×40min 2nd Vulcanization 150℃×2Hr |
|