Order Test Name Result Exam Conditions
1 State
Physical
Properties
Hardness(HS) 67 170℃×6min
Tensile Strength(Kgf/㎠) 155.89
Elongation Rate(%) 324.4
2 Heat
Resistance
Test
Hardness Change Rate(HS) 6 100℃×70hrs
Tensile Strength Change Rate(%) 0.1%
Elongation Rate Change(%) -25.09%
3 Oil
Resistance
Test
Hardness Change Rate(HS) 8 100℃×70hrs
NO1
Tensile Strength Change Rate(%) 3.7%
Elongation Rate Change(%) -19.24%
Modulus of Volume Change(%) -8.33%
Modulus of Volume Change(%) 2.13% 100℃×70hrs
NO3
Compression Permanent Shrinkage Rate(%) 4.9% 100℃×22hrs×25%
4 Cold Resistance(TR 10) -42.2