| Order | Test Name | Result | Exam Conditions | |
|---|---|---|---|---|
| 1 | State Physical Properties |
Hardness(HS) | 69 | 170℃×6min |
| Tensile Strength(Kg/㎠) | 159 | |||
| Elongation Rate(%) | 327 | |||
| 2 | Heat Resistance Test |
Hardness Change Rate(HS) | 7 | 120℃×70hrs |
| Tensile Strength Change Rate(Kg/㎠) | -3.1% | |||
| Elongation Rate Change(%) | -37.6% | |||
| 3 | Oil Resistance Test |
Hardness Change Rate(HS) | 3 | 120℃×70hrs NO1 |
| Tensile Strength Change Rate(Kg/㎠) | -4.4% | |||
| Elongation Rate Change(%) | -30.6% | |||
| Modulus of Volume Change(%) | -4.3% | |||
| Hardness Change Rate(HS) | -10 | 120℃×70hrs NO3 |
||
| Tensile Strength Change Rate(Kg/㎠) | -78% | |||
| Elongation Rate Change(%) | -58.1% | |||
| Modulus of Volume Change(%) | 21.5% | |||
| 4 | Compression Permanent Shrinkage Rate(%) | 9.7% | 120℃×22hrs Production 170℃ * 40min |
|